ASTM A335 P22 Seamless Ferritic Alloy-Steel Pipe
Description
ASTM A335 P22 Seamless Ferritic Alloy-Steel Pipe
Standard:ASTM A 335/A 335M
Standard Specification for Seamless Ferritic Alloy-Steel Pipe for High-Temperature Service
ASTM A335 P22 Seamless Ferritic Alloy-Steel Pipes cover nominal (average) wall seamless alloy-steel pipe intended for high-temperature service.
ASTM A335 P22 Steel
Equivalent steel grade
Grade | Standard | Country |
STBA24 | JIS G3462 | Japan |
10CrMo910 | DIN 17175 | Germany |
12Cr2MoG | GB/T 5310 | China |
Heat Treatment:
Grade P22 Seamless Ferritic Alloy-Steel Pipe will be reheated and furnished in the full-annealed, isothermal annealed, or normal-ized and tempered condition. If furnished in the normalized and tempered condition, the minimum tempering temperature are 1250°F [675°C].
Chemical Composition of ASTM A335 P22
Grade | Chemical Composition(%) | ||||||
C | Mn | P | S | Si | Cr | Mo | |
P22 | ≤0.015 | 0.30-0.60 | ≤0.025 | ≤0.025 | ≤0.50 | 1.90-2.60 | 0.87-1.13 |
Mechanical Properties of ASTM A335 P22
Grade | Mechanical property | ||
Tensile Strength(MPa) | Yield Strength(MPa) | Elongation(%) | |
P22 | ≥415 | ≥205 | ≥30 |
Outside diameter tolerances of ASTM A335 Seamless Ferritic Alloy-Steel Pipe
NPS Designator | Over | Under | ||
in. | mm | in. | mm | |
1⁄8 to 1 1⁄2 , incl. | 1 ⁄ 64 (0.015) | 0.40 | 1 ⁄ 64 (0.015) | 0.40 |
Over 1 1⁄2 to 4, incl. | 1 ⁄ 32 (0.031) | 0.79 | 1 ⁄ 32 (0.031) | 0.79 |
Over 4 to 8, incl. | 1 ⁄ 16 (0.062) | 1.59 | 1 ⁄ 32 (0.031) | 0.79 |
Over 8 to 12, incl. | 3 ⁄ 32 (0.093) | 2.38 | 1 ⁄ 32 (0.031) | 0.79 |
Over 12 | ± 1 % |